Selenium, Sulfur
Copper, Lead, Silver
Browner than in the struck sheet, the color matures to golden green during the firing process.
May reveal subtle light/dark green wisps in a full-fuse firing. When uncapped, the mottling is less noticeable and the color more even. When capped with clear, the mottling is more noticeable.
This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.